Modeling and Numerical Solution of Galvanic Corrosion of Marine Structures
"Modeling and Numerical Solution of Galvanic Corrosion of Marine Structures"
4th International Conference in Coasts, Ports and Marine Structures, (ICOPMAS 2000), Iran, Nov. 2000.
Abbstract :